High-dose ion implantation of phosphorus into 4H-SiC has been investigated. Phosphorus ion implantation with a 1x10(16) cm(-2) dose at 800 degreesC into 4H-SiC (0001) has resulted in a sheet resistance of 80 Omega/square after annealing at 1700 degreesC. A similar sheet resistance of 110 Omega/square was achieved even by room-temperature implantation when 4H-SiC (11 (2) over bar0) was employed, owing to excellent recrystallization of this face revealed by Rutherford backscattering channeling spectroscopy. The sheet resistance could be further reduced down to 27 Omega/square by 800 degreesC implantation into 4H-SiC (11 (2) over bar0) followed by annealing at 1700 degreesC. 4H-SiC (11 (2) over bar0) showed a very flat surface after annealing. (C) 2002 American Institute of Physics.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据