Effects of fuel impurities on the fireside corrosion of boiler tubes in advanced power generating systems - a thermodynamic calculation of deposit chemistry

期刊

CORROSION SCIENCE
卷 44, 期 2, 页码 265-283

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/S0010-938X(01)00060-9

关键词

high temperature corrosion; fireside corrosions; boiler tube materials; hot corrosion

向作者/读者索取更多资源

Thermodynamic equilibrium calculation relating fuel chemistry with flue-gas composition and volatile condensate deposits on tube metals upon combustion of various dirty fuel was conducted for a better understanding of the deposit chemistry of superheater tubes in steam-generating boilers. Corrosive impurities such as sodium. potassium, chlorine, and sulfur. inevitably involved in fuel. were considered in the calculation. Possible influence of flue-gas temperature on deposit chemistry was investigated as well. Based on the flue-gas composition and the deposit chemistry, corrosion environments of steam-generating boilers firing various dirty fuel were discussed. (C) 2001 Elsevier Science Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据