Seven hemicellulosic preparations were obtained from barley straw by extraction with 1.5% H2O2 at pH 12.0 for 14h at 45degreesC with extractant to straw ratios of 10:1, 13:1, 15:1, 18:1, 20:1, 25:1 and 30:1. The respective yields of dissolved hemicelluloses were 28.4 wt%, 28. 8 wt%, 29.7 wt%, 30.1 wt%, 30.6 wt%, 30.8 wt% and 30.8 wt% or dry barley straw, corresponding to release of 78.7%, 79.8%, 82.3%, 83.4%, 84.8%, 85.3% and 85.3% of the original hemicelluloses. The polymers were mainly composed of xylose, arabinose, glucose, galactose and 4-0-methyl-D-glucuronic acid (59.3-62.6%, 19.7-22.0%, 8.8-12.5%, 5.6-6.9% and 5.8-6.7%, respectively) and had weight-average molecular weights of between 38 470 and 41 050 g mol(-1). (CNMR)-C-13 spectroscopy confirmed the results obtained by chemical methods, and showed that the hemicellulosic fraction was mostly by L-arabino-(4-0-methyl-D-glucurono)-D-xylan. More importantly, it was found that lignin provides some protection for the hemicelluloses in barley straw against attack by hydrogen peroxide. (C) 2002 Society of Chemical Industry.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据