The influence of temperature on the wear mode and deterioration of coatings used for titanium aircraft engine components

期刊

TRIBOLOGY TRANSACTIONS
卷 45, 期 2, 页码 193-198

出版社

TAYLOR & FRANCIS INC
DOI: 10.1080/10402000208982539

关键词

fretting; wear; dovetail; titanium; coatings

向作者/读者索取更多资源

The interface between titanium compressor blades and rotors of jet engines was studied to determine the mechanisms responsible for problematic deteriorations of protective Cu-Ni-In coatings. Results indicated that at operational temperatures of 221degreesC, titanium from the uncoated disk was transferred to the softer Cu-Ni-In coating on the blade. This in turn created titanium on titanium contact and resulted in fretting wear. At higher temperatures of 454degreesC, copper segregation appears to be the dominant deterioration mechanism. In order to simulate these wear modes and evaluate candidate coatings, a unique testing procedure was developed that included a range of gross-slip scale displacements. Cobalt, molybdenum, tungsten carbide, and Nickel-based coatings were evaluated by this testing procedure that first involved a low-cycle series of gross-slip displacements (125 mum), followed by a higher cycle series in a reduced (25 mum) gross-slip regime. Results of the study revealed that an unlubricated pure-cobalt coating could protect the blade without damaging the disk at elevated temperatures. While no coatings performed exceptionally at lower temperatures, pure molybdenum exhibited some promise.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据