This study compares the behaviour of aluminium in the bare condition and when protected with anodic films of approximately 7, 17 and 28,m thickness for up to 42 months of exposure in 11 atmospheres of very different aggressivities, with salinity values ranging between 2.1 and 684 mg Cl- m(-2) d(-1). The results of a previous study based on visual inspection and traditional gravimetric techniques are complemented by the application, essentially, of electrochemical impedance spectrascopy (EIS). The specimens were characterised by EIS when recently obtained and after 12, 24 and 42 months of exposure in the different testing stations. Exposure leads to an improvement in ail the quality indices of anodic films, irrespective of their thickness or the degree of environmental pollution. Anodising and sealing prevents localised corrosion - which is characteristic of aluminium in marine or industrial atmospheres - even in the most unfavourable situations, except in the case of 7 p,m films, the lowest thickness tested. (C) 2002 Elsevier Science B.V All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据