A higher conductivity Bi2O3-based electrolyte

期刊

SOLID STATE IONICS
卷 150, 期 3-4, 页码 347-353

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/S0167-2738(02)00291-6

关键词

bismuth oxide; polarizability; double doping; structural stability; electrical conductivity

向作者/读者索取更多资源

We have developed a Bi2O3 electrolyte doped with Dy2O3 and WO3 (DyWSB) that exhibits a higher conductivity than that of 20 mol% erbia stabilized bismuth oxide (20ESB), thus, giving it the highest conductivity of any known solid oxide electrolyte. Electrical conductivity results of the Dy-W stabilized bismuth oxide system are presented. The dopants were selected based on their polarizability and its effect on structural stability and conductivity. At 800 degreesC, the conductivity of (BiO1.5)(0.88)(DyO1.5)(0.08)(WO3)(0.04) is 0.57 S/cm (1.5 times as high as that of 20ESB), and at 500 degreesC, the conductivity is 0.043 S/cm (2 times as high as that of 20ESB). (C) 2002 Elsevier Science B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据