The effect of synthetic conditions on tailoring the size of hydrotalcite particles

期刊

SOLID STATE IONICS
卷 151, 期 1-4, 页码 285-291

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/S0167-2738(02)00725-7

关键词

hydrotalcite; particle size; crystal growth; urea hydrolysis

向作者/读者索取更多资源

The hydrotalcite particles Of Mg2Al(OH)(6)(CO3)(1/2).0.1H(2)O have been prepared by two different methods: (1) direct coprecipitation of aqueous solution of Mg(NO3)(2).6H(2)O, Al(NO3)(3).9H(2)O upon hydrolysis of urea, and (2) hydrothermal aging of the same nitrate solution after NaOH titration. In order to control the particle size and morphology of hydrotalcite, various parameters such as metal ion concentration, aging time, reaction temperature are systematically studied. According to the powder X-ray diffraction, all the samples turn out to be well crystallized with an average basal spacing of 7.6 Angstrom corresponding to the hydrotalcite crystal. From the SEM images, the coprecipitates are found to be hexagonal in shape and are controlled in the particle size range of 0.9-2.2 and 1.2-4.5 mum depending on aging time (6-69 h) and metal ion concentration (0.87-0.065 M), respectively. However, the particle size of the hydrothermally prepared samples increase in proportion to aging time (12 - 72 h; 85-120 nm) and reaction temperature (100-180 degreesC 115-340 nm). The effect of such parameters upon the particle size was rationalized on the basis of crystal growth mechanism. (C) 2002 Elsevier Science B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据