4.3 Review

Fracture reasons in ceramic-fused-to-metal restorations

期刊

JOURNAL OF ORAL REHABILITATION
卷 30, 期 3, 页码 265-269

出版社

WILEY
DOI: 10.1046/j.1365-2842.2003.01038.x

关键词

fracture; ceramics

向作者/读者索取更多资源

Ceramic-fused-to-metal restorations are widely used in dentistry with a high degree of general success. Fracture of the ceramic veneers as a result of oral function or trauma is not an uncommon problem in clinical practice. Although fractures of such restorations do not necessarily mean the failure of the restoration, the renewal process is both costly and time consuming and therefore remains a clinical problem. Fractures in the anterior region pose an aesthetic problem but when they are in the posterior, chewing function could also be affected. The published literature reveals that reasons for failures cover a wide spectrum from iatrogenic factors to laboratory mistakes or because of factors related to the inherent structure of the ceramics or simply to trauma.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据