Combination of mechanical alloying and two-stage sintering of a 93W-5.6Ni-1.4Fe tungsten heavy alloy

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/S0921-5093(02)00410-0

关键词

tungsten heavy alloy; mechanical alloying; two-stage sintering; microstructural parameter; mechanical properties

向作者/读者索取更多资源

The microstructural evolution and mechanical properties of a mechanically alloyed and two-stage sintered tungsten heavy alloy were investigated. Elemental powders of tungsten, nickel and iron of a composition corresponding to 93W-5.6Ni-1.4Fe were mechanically alloyed in a tumbler ball mill for 72 h. Mechanically alloyed powders were solid-state sintered at 1300 degreesC for 1 hr in a hydrogen atmosphere followed by secondary sintering at 1445-1485 degreesC for a sintering time ranging from 4 to 90 min. Solid-state sintered tungsten heavy alloys exhibited full densification (above 99% in relative density) due to the enhanced sintering resulting from mechanical alloying. Secondary sintering with a rapid heating rate changed the microstructures of the solid-state sintered alloy with contiguous tungsten phases into a dispersion alloy with spherical tungsten particles embedded in the W-Ni-Fe matrix, maintaining fine tungsten particle due to the combination of a mechanical alloying and a short sintering time. The two-stage sintered tungsten heavy alloy from mechanically alloyed powders showed finer tungsten particle (about 6 mum in diameter) than in conventional liquid-phase sintered tungsten heavy alloys. The mechanical properties of a tungsten heavy alloy were found to be dependent on the microstructural parameters such as tungsten particle size, matrix volume fraction and tungsten/tungsten contiguity which are controllable through the two-stage sintering process. (C) 2002 Elsevier Science B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据