silicon; magnesium; substitution; hydroxyapatite; sintering behavior
Si, Mg-substituted hydroxyapatites, alone and co-substituted, have been prepared to obtain biomaterials having an improved biocompatibility, From FT-IR, XRD and ICP analyses, it was confirmed that single phases of hydroxyapatite substituted by Si alone or co-substituted by Si, Mg. The XRD data indicated the absence of extra phases related to silicon and magnesium oxide or other calcium phosphate species. Si-substituted hydroxyapatite of up to 2 wt% for Si and Si, Mg co-substituted hydroxyapatite of 1 wt% for the each ion keep their original structures intact for the sintering temperatures of up to 1200degreesC. However, it is observed that ion substitutions by an amount higher than the above ratios for each hydroxyapatite lead to destabilization of original structures of the hydroxyapatite and to the production of tricalcium phosphate and calcium phosphate silicate phases when the samples were sintered at 1100degreesC or higher. (C) 2002 Elsevier Science Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据