Oxygen transfer in BIMEVOX materials

期刊

SOLID STATE IONICS
卷 160, 期 1-2, 页码 85-92

出版社

ELSEVIER
DOI: 10.1016/S0167-2738(03)00142-5

关键词

fast oxide ion conductors; oxygen diffusion; surface exchange; bismuth-based materials

向作者/读者索取更多资源

Two steps govern the oxygen transport in ceramic oxide ion conductors: (i) the oxygen exchange at the surface of the material and (ii) the oxygen diffusion through the material. The O-18/O-16 Isotope Exchange Depth Profile technique (IEDP) was applied to BIMEVOX materials to characterise the oxygen transfer in these ceramics. The isotope concentration profiles, obtained by secondary ion mass spectrometry (SIMS), revealed that the equilibrium exchange kinetics in BIMEVOXes under nominally dry oxygen are dominated by a relatively slow surface exchange step. This produces deep penetration profiles with very low isotopic concentrations close to the natural isotopic background. The oxygen surface exchange coefficient in these materials is of the same order of magnitude as in the classical oxide electrolytes, ceria gadolinia (CGO) and yttria-stabilised zirconia (YSZ). The transfer of oxygen from water is far easier, which makes the accurate determination of the true coefficient of exchange of the molecular oxygen for these materials more complicated and is probably dominated by the presence of residual water. (C) 2003 Published by Elsevier Science B.V.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据