4.6 Article

A morphological and micro-tensile bond strength evaluation of a single-bottle adhesive to caries-affected human dentine after four different caries removal techniques

期刊

JOURNAL OF DENTISTRY
卷 31, 期 6, 页码 429-435

出版社

ELSEVIER SCI LTD
DOI: 10.1016/S0300-5712(03)00011-3

关键词

dentin bonding; demineralized dentin; human carious dentin; hema; SEM; strength; adhesion; resin; Adhesive Systems; layer

向作者/读者索取更多资源

Objectives. This study evaluated the influence of different caries removal techniques (conventional bur; chemomechanical removal/Carisotv(TM)-MediTeam; a sonic preparation system/SonicsysMicro-Kavo and air abrasion/PrepStar-Danville Engineering) on microtensite bond strength to caries-affected human dentine. Methods. Occlusal. surfaces of extracted human permanent third molars with coronal dentine caries extending approximately halfway through the dentine was ground perpendicular to the long axis of the tooth to expose a flat surface of normal dentine surrounding the carious lesion with laser fluorescence values of approximately 30 (DIAGNODent(R), KaVo). Carious lesions were excavated with one of the four techniques until laser fluorescence values decreased to 15 in the center of the lesions. An ethanol-based dentine adhesive (Single Bond, 3M) was used to bond composite resin (P60, 3M) to the substrate. Vertical slices (n = 11/group), approximately 0.8 mm thick were made through the caries-affected portions of each tooth, perpendicular to the bonding surface. Specimens were subjected to tensile stress at a crosshead speed of 1 mm/min. Data were analyzed by Kruskal-Wallis test. SEM investigation was performed for the qualitative evaluation of resin-dentine hybridization. Results. The microtensite bond strengths were as follows (mean +/- SD in MPa): 6.4 +/- 5.3 (bur), 8.4 +/- 3.3 (Carisolv), 8.5 +/- 5.9 (Sonicsys Micro), and 8.8 +/- 8.8 (air abrasion). Statistical analysis did not show significant differences between any of the treatment modalities (p = 0.160). Tensile fracture was cohesive within caries-affected dentine in all specimens. Conclusions. The four different caries removal techniques used within this study did not influence the bond strength of the tested dentine adhesive to caries-affected human dentine. (C) 2003 Elsevier Science Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据