4.7 Article

The glass transition and interfacial layer in styrene-butadiene rubber containing silica nanofiller

期刊

POLYMER
卷 44, 期 20, 页码 6259-6266

出版社

ELSEVIER SCI LTD
DOI: 10.1016/S0032-3861(03)00667-0

关键词

nanofiller; composite; mechanical relaxation

向作者/读者索取更多资源

The mechanical behaviour of a styrene-butadiene rubber, containing 23.5% styrene and filled with up to 55% by weight with silica nanoparticles, has been examined. The tan 5 spectra of these composites show a second relaxation of relatively low intensity located about 40 degreesC above the main a relaxation, the glass transition T-g, which occurs at -34.5 degreesC in the unfilled polymer. This is attributed to an interfacial layer of polymer molecules whose chain relaxation dynamics have been altered by interaction with the filler surface. This is accompanied by a shift of the T-g itself to lower temperature when the filler surface is organophilic, but not when the filler surface is hydrophilic, and possible mechanisms for this are discussed. The amount of interfacial polymer can be quantified by resolving the glass transition and the second relaxation using a curve-fitting approach. A first-order treatment is presented which estimates the layer thickness to be of the order of a few nanometers. (C) 2003 Published by Elsevier Ltd.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据