4.6 Article Proceedings Paper

Electrocatalysis in water electrolysis with solid polymer electrolyte

期刊

ELECTROCHIMICA ACTA
卷 48, 期 25-26, 页码 3945-3952

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.electacta.2003.04.001

关键词

electrocatalysis; water electrolysis; oxygen electrode; iridium oxide; solid polymer electrolyte

向作者/读者索取更多资源

Powders of IrO2 were used as anode catalysts in water electrolysis cells with solid polymer electrolyte (SPE). The catalyst was prepared by a pyrolysis process in a nitrate melt at 340 degreesC and then annealed at different temperatures from 440 to 540 degreesC. The catalyst materials were applied to an electrode membrane assembly (MEA) and studied in situ in an electrolysis cell using cyclic voltammetry (CV), electrochemical impedance spectroscopy (EIS) and stationary current density-potential relations. The impedance results clearly show that the non-annealed material possesses the highest electrocatalytic activity and that this activity deteriorates with increasing annealing temperature. The electrical conductivity, however, increases by increasing annealing temperature. Optimum annealing conditions were found at 490 C, where the total polarisation reaches a minimum in the high current density range (1-2 A cm(-2)), at the actual conditions. Increased crystallinity and size of the particles with increasing annealing temperature was observed by transmission electron microscopy (TEM). A very high electrochemical performance was obtained in a water electrolysis cell using IrO2 on the anode side and Pt on Vulcan XC-72 on the cathode side, corresponding to a current density of 1 A cm(-2) at 1.60 V. (C) 2003 Elsevier Ireland Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据