Our previous work applied a novel supported iron oxyhydroxide (FeOOH) catalyst to effectively treat benzoic acid by hydrogen peroxide. The FeOOH catalyst was prepared via the oxidation of Fe2+ by H2O2 in the acidic condition using a fluidized-bed crystallization reactor. The major components coated on the surface were identified as amorphous FeOOH and gamma-FeOOH. In terms of the crystallization conditions of FeOOH, some parameters including the operational pH, superficial velocity, specific iron loading, and influent H2O2 concentration were investigated to quantify their effects on the crystallization efficiency. All these parameters were found to significantly influence the crystallization efficiency. Two types of FeOOH catalysts were synthesized: FeOOH I was prepared at pH 3.5, and FeOOH 11 was formed by aging FeOOH I at pH 13. The percentages of surface amorphous FeOOH reduced from 70% to 30% after aging. The FeOOH 11 catalyst presented a higher reactivity toward H2O2 but lower stoichiometric efficiency in oxidizing benzoic acid than FeOOH 1, similar to the result of the commercial goethite. Therefore, it is concluded that the crystalline property significantly affects the performance of catalytic oxidation. (C) 2003 Elsevier Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据