Chemical degradation of fluoroelastomer in an alkaline environment

期刊

POLYMER DEGRADATION AND STABILITY
卷 83, 期 2, 页码 195-206

出版社

ELSEVIER SCI LTD
DOI: 10.1016/S0141-3910(03)00235-0

关键词

chemical degradation; FKM (Viton A ); fluoroelastomer; XPS and ATR-FTIR; mechanical properties

向作者/读者索取更多资源

We have investigated the time-dependent chemical degradation of a fluoroelastomer, FKM (Viton((R)) A), in an alkaline environment (10% NaOH, 80 degreesC). Optical microscopy and SEM analysis reveal that degradation starts with surface roughness right from the earliest stage of exposure (e.g., 1 week) and finally results in cracks on the surface after prolonged exposure. Initially the extent of degradation is mainly confined to the surface regions (a few nanometers) but with longer exposure (e.g., 12 weeks) it extends to below the subsurface region of the fluoroelastomer. The extent of this surface degradation is found to be strong enough to affect the bulk mechanical properties. The molecular mechanisms of the surface chemical degradation were determined using surface analysis (XPS and ATR-FTIR) where the initial degradation was found to proceed via dehydrofluorination. This leads to double bond formation on the rubber backbone which accelerates the degradation even further with longer exposure. Furthermore, the cross-link sites of the exposed rubber samples are also found to be vulnerable to hydrolytic attack under the studied chemical environment as evidenced by the decrease in cross-link density and gel fraction (%). (C) 2003 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据