Layered basic zinc acetate (LBZA), Zn-5(OH)(8)(CH3COO)(2).2H(2)O, was deposited on glass substrates by a chemical bath deposition (CBD) method using methanolic solutions of zinc acetate dihydrate. The substrates were put into bottles filled with the solutions and sealed up and were kept at 60 degreesC in a drying oven. Immersion time necessary for the deposition of LBZA films was typically more than 28 h. This was a key to inducing heterogeneous nucleation of LBZA through control over a degree of supersaturation in the evolution of a unique, nest-like morphology. Hydration water contained by zinc acetate dihydrate was quantitatively enough to promote hydrolysis of zinc acetate. The LBZA films were transformed into nanocrystalline, porous ZnO films without morphological deformation by heating at 150 degreesC in air. A mechanism of the formation of the nest-like morphology was discussed based on nonaqueous solution reactions, nucleation, and crystal growth during the CBD process. (C) 2003 Elsevier Inc. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据