4.7 Article

Buckle delamination on patterned substrates

期刊

ACTA MATERIALIA
卷 52, 期 10, 页码 3151-3159

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.actamat.2004.03.014

关键词

films; buckling; adhesion; lithography; interface toughness

向作者/读者索取更多资源

Lithographic techniques applied to a substrate prior to film deposition can create areas of low interface adhesion surrounded by regions of high adhesion. If the film is under compression and if buckle delamination is nucleated, conditions can be controlled such that delaminations are confined to the patterned areas of low adhesion. When the area of low adhesion is a strip, the width of the strip controls the buckle morphology: smooth Euler buckles for narrow strips, asymmetric telephone cord buckles for wider strips, and symmetric varicose buckles under a very limited range of conditions. Results for the elastic energy in the buckled state show that above a critical stress the telephone cord morphology is the preferred morphology. Energy release rates for propagating delaminations are determined for each of the three morphologies. Tapered strips provide an accurate means of measuring interface adhesion based on the width of the strip where the delamination arrests. (C) 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据