期刊
CEMENT AND CONCRETE RESEARCH
卷 34, 期 7, 页码 1167-1172出版社
PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.cemconres.2003.12.023
关键词
silica fume; microstructure; composites; bond strength; pullout strength; interfacial transition zone
In this paper, the effect of silica fume on the bond characteristics of steel fiber in matrix of reactive powder concrete (RPC), including bond strength, pullout energy, etc., are presented. The experimental results on steel fiber pullout test of different conditions are reported. Various silica fume contents ranging from 0% to 40% are used in the mix proportions. Fiber pullout tests are conducted to measure the bond characteristics of steel fiber from RPC matrix. It is found that the incorporation of silica fume can effectively enhance the fiber-matrix interfacial properties, especially in fiber pullout energy. It is also concluded that in terms of the bond characteristics, the optimal silica fume content is between 20% and 30%, given the conditions of the experimental program. The microstructural observation confirms the findings on the interfacial-toughening mechanism drawn from the fiber pullout test results. (C) 2004 Elsevier Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据