Preparation and characterization of a novel Si-incorporated ceramic film on pure titanium by plasma electrolytic oxidation

期刊

APPLIED SURFACE SCIENCE
卷 254, 期 16, 页码 5216-5223

出版社

ELSEVIER
DOI: 10.1016/j.apsusc.2008.02.047

关键词

titanium; plasma electrolytic oxidation; ceramic film; bioactivity; apatite

向作者/读者索取更多资源

A Si-incorporated bioactive ceramic film was prepared on pure titanium by plasma electrolytic oxidation (PEO) in a new bath containing Ca2+, H2PO4- and SiO32-. The film was characterized by scanning electron microscopy (SEM), X-ray diffraction (XRD) and X-ray photoelectron spectroscope (XPS). The apatite-induced ability of PEO film was evaluated by soaking in a simulated body fluid (SBF) for various periods. The results showed that Si-incorporated PEO film present a porous microstructure, the pore size is around 1-5 mu m. The film mainly consists of anatase and rutile and a small amount of CaHPO4 and CaO, besides, bioactive compounds such as CaSiO3 and SiO2, also exist in the Si-incorporated PEO film. After immersion in SBF for 28 days, not only the surface layer but also the pores inside the Si-incorporated PEO film were completely filled by apatite crystals, whereas on the surface of a benchmark PEO film free of Si just present small piles of apatite crystals. Silicon incorporated into the PEO film provided more heterogeneous nucleation sites for apatite deposition and hence increased remarkably bioactivity of the PEO film. (C) 2008 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据