4.8 Article

Fatigue characteristics of bioactive glass-ceramic-coated Ti-29Nb-13Ta-4.6Zr for biomedical application

期刊

BIOMATERIALS
卷 25, 期 17, 页码 3369-3378

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.biomaterials.2003.09.108

关键词

titanium alloys; biomaterials; bioactive coating; fatigue

向作者/读者索取更多资源

A new surface-coating method by which CaP invert glass is used to improve the bioactivity of titanium alloys has been developed recently. In this method, the powder of CaP invert glass (CaO-P2O5-TiO2-Na2O) is coated on the surface of titanium alloy samples and heated between 1073 and 1123 K. With this treatment, a calcium phosphate layer mainly containing beta-Ca-3(PO4)(2) phase can be coated easily on titanium alloy samples. In the present study, the effect of this coating process on the fatigue properties of Ti-29Nb-13Ta-4.6Zr, a new metastable beta alloy for biomedical applications, has been investigated. The fatigue endurance limit of the coated alloy was found to be about 15% higher than that of uncoated alloy, as a result of the formation of a hard (alpha + beta) layer and a small amount of the omega phase during the coating process. The coating exhibits excellent adhesion to the substrate during the tensile and fatigue tests. Subsequent ageing at 673 K for 259.2 ks greatly improves the fatigue resistance of the coated alloy due to isothermal omega phase precipitation, and does not have obvious detrimental effect on the coating properties. (C) 2003 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据