Yield strength and strain hardening of MgO up to 8 GPa measured in the deformation-DIA with monochromatic X-ray diffraction

期刊

EARTH AND PLANETARY SCIENCE LETTERS
卷 226, 期 1-2, 页码 117-126

出版社

ELSEVIER
DOI: 10.1016/j.epsl.2004.07.023

关键词

deformation; initial yield strength; flow stress; strain hardening; lattice strain

向作者/读者索取更多资源

Cylindrical polycrystalline MgO samples have been deformed with total axial strains up to 35% at pressures up to 8 GPa. Hysteresis loops between elastic lattice strain and total axial strain were established by repeatedly shortening and lengthening the samples at selected strain rates. The yield point was identified as the first deviation from linearity in the lattice strain versus total strain curves. MgO samples yielded at low total strains (< 1%) and the yield strength (ca. 0.5 GPa) was insensitive to pressure. Beyond the yield point, MgO showed a strong strain-hardening behavior, characterized by an initial rapid increase in flow stress, followed by a linear stage with a constant hardening parameter. At pressures below 5 GPa, lattice strains associated with reflections 200, 220, and 222 diverged with increasing total strain. Above 5 GPa, these lattice strains converged, suggesting a possible change in flow mechanism. (C) 2004 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据