The effect of thermal annealing on photovoltaic devices comprising poly(3-hexylthiophene):[6,6]-phenyl C-61 butyric acid methyl ester (P3HT:PCBM) with thicknesses up to 1200 nm was investigated. Without thermal annealing, the efficiency of the as-prepared devices decreased with increasing active layer thickness, reflecting largely a reduction in the short-circuit current density and an inverse photocurrent spectral response. Thermal annealing of the full devices was found to substantially recover thick-film device efficiencies while reducing the thin-film device efficiencies. The profound variations in photovoltaic characteristics were interpreted in terms of vertical phase separation in the P3HT: PCBM blend film and Li+ diffusion from the LiF/Al contact. (C) 2010 American Institute of Physics. [doi: 10.1063/1.3474654]

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据