Temperature dependence of resistivity, dielectric constant and dielectric loss have been investigated for four different compositions of nickel-zinc ferrites, Ni1-xZnxFe2O4 (x = 0.2, 0.35, 0.5 and 0.6), prepared by the citrate precursor technique. Activation energies calculated from the resistivity versus temperature curves for the compositions sintered at 1200degreesC and 1300degreesC range from 0.55 eV to 0.73 eV. Samples sintered at 1200degreesC exhibit higher activation energies and low dielectric losses compared to those sintered at 1300degreesC. Samples of the composition with x = 0.6 show low dielectric losses up to a measurement temperature of around 200degreesC at higher frequencies as compared to samples of other compositions. The variations in activation energy with composition and sintering temperature have been explained on the basis of the site occupancy in ferrites and the atomic radii of the constituent metal ions. (C) 2004 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据