4.4 Article

Copper compatible barium titanate thin films for embedded passives

期刊

JOURNAL OF ELECTROCERAMICS
卷 14, 期 2, 页码 95-102

出版社

SPRINGER
DOI: 10.1007/s10832-005-0866-6

关键词

barium titanate; copper; ferroelectric; film; capacitor

向作者/读者索取更多资源

Barium titanate thin films have been prepared by chemical solution deposition on 18 mu m thick, industry standard copper foils in the absence of chemical barrier layers. The final embodiment exhibits randomly oriented BaTiO3 grains with diameters between 0.1 and 0.3 mu m, and an equiaxed morphology. The average film thickness is 0.6 mu m and the microstructure is free from secondary or interfacial phases. The BaTiO3 films are sintered in a high temperature reductive atmosphere such that copper oxidation is avoided. Subsequent lower-temperature, higher oxygen pressure anneals are used to minimize oxygen point defects. Permittivities of 2500 are observed at zero bias and room temperature, with permittivities greater than 3000 at the coercive field. Loss tangents under 1.5% are demonstrated at high fields. The BaTiO3 phase exhibits pronounced ferroelectric switching and coercive field values near 10 kV/cm. Temperature dependent measurements indicate a ferroelectric transition near 100 degrees C with very diffuse character. Combining the approaches of the multilayer capacitor industry with traditional solution processed thin films has allowed pure barium titanate to be integrated with copper. The high sintering temperature - as compared to typical film processing - provides for large grained films and properties consistent with well-prepared ceramics. Integrating BaTiO3 films on copper foil represents an important step towards high capacitance density embedded passive components and elimination of economic constraints imparted by traditional noble metallization.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据