Characteristic changes of deuterium retention on tungsten surfaces due to low-energy helium plasma pre-exposure

期刊

JOURNAL OF NUCLEAR MATERIALS
卷 337, 期 1-3, 页码 927-931

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jnucmat.2004.10.011

关键词

deuterium retention; helium; NAGDIS-II; tungsten

向作者/读者索取更多资源

Deuterium retention in tungsten increases substantially when it is pre-exposed to low-energy He plasma at a high temperature (1600 K), while it decreases when pre-exposed at a low temperature (700 K). The increase of deuterium retention could be attributed to the submicron-sized He bubbles and secondary interstitial defects formed on the tungsten surface. Occupation of trap sites by He atoms during the He pre-exposure at low temperature could decreases the effective number of available trap sites for deuterium atoms, which would decreases the deuterium retention on the tungsten surface. (c) 2004 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据