期刊
SOLID STATE IONICS
卷 176, 期 9-10, 页码 895-903出版社
ELSEVIER SCIENCE BV
DOI: 10.1016/j.ssi.2004.10.024
关键词
Li-secondary battery; layered oxides; synchrotron XRD measurement; XAFS measurement; SQUID measurement; maximum entropy method
Structural changes in Li1-yNi0.5Mn0.5O2 With Li de-intercalation were studied using X-ray diffraction, XAFS, and magnetic measurements. The Li de-intercalation from LiNi0.5Mn0.5O2 proceed mainly by a valence state change of Ni ions from Ni2+ to Ni3+ Up to y=0.5 from the XANES and magnetic results. Structural analysis clarified that a second order phase transition from trigonal to monoclinic was observed between Y=0.2 and 0.3 and that a small fraction of the Li ions start to migrate from the octahedral 2a site to the tetrahedral 4i site at y=0.3 and most of the Li ions occupied the tetrahedral 4i site at y=0.5 with Li de-intercalation. The EXAFS analysis clarified the valence state change and the range of phase transition during the Li de-intercalation, from the changes in the bond distance of the first neighbor for each transition metal. This Li de-intercalation mechanism is characteristic of this system and has not been reported for Li1-yMO2 (M=Co and Ni). (c) 2004 Elsevier B.V. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据