4.7 Article

Thermal degradation and pyrolysis of mixtures based on poly(3-hydroxybutyrate-8%-3-hydroxyvalerate) and cellulose derivatives

期刊

POLYMER TESTING
卷 24, 期 4, 页码 526-534

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.polymertesting.2004.11.013

关键词

thermal degradation; poly(3-hydroxybutyrate-co-3-hydroxyvalerate); cellulose; thermogravimetric analysis; Pyrolysis-GC-MS

向作者/读者索取更多资源

Thermal degradation and pyrolysis behaviour of mixtures based on poly(3-hydroxybutyrate-co-8%-3-hydroxyvalerate) (P(HB-8%HV)) and cellulose derivatives has been studied. The effect of the formulation of mixtures in the thermal degradation of both co-components was evaluated. TG/DTG experiments and Py-GC-MS were used in this study. Solid-solid and gas-solid interactions between co-components were analyzed by using a simple mixture rule. Mixtures with microcrystalline cellulose (MC) resulted in an enhancement of thermal stability of both co-components due to strong hydrogen type interactions in the solid state and between gases evolved from polymer decomposition and solid MC. Crotonic acid seemed to induce a higher order in cellulose, causing disruption of some hydrogen bonds within it and promoting the formation of more stable cellulose structure. On the other hand, sisal fiber showed an unfavourable effect on polymer thermal stability. Acetic acid produced from hemicellulose thermal decomposition seemed to act as acid promoter for the random scission of ester linkages in P(HB-8%HV). (c) 2005 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据