Enzymatic degradation of PLLA-PEOz-PLLA triblock copolymers

期刊

BIOMATERIALS
卷 26, 期 16, 页码 2803-2811

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.biomaterials.2004.07.064

关键词

PLLA-PEOz-PLLA; proteinase k; biodegradable; enzymatic degradation

向作者/读者索取更多资源

The enzymatic degradation of poly(L-lactide)-block- poly(2-ethyl-2-oxazoline)-block-poly(L-lactide) triblock copolymer (PLLA-PEOz-PLLA) was investigated using efficient enzyme proteinase K. PLLA-PEOz-PLLA solution-cast film lost a considerable amount of hydrophilic copolymers in the first 2 h, and the degradation after 2 h proceeded predominantly by surface erosion. The two faces of the hydrolyzed film exhibited different morphologies following enzymatic degradation. The lower face showed many spherulites, which are the superstructural morphology of polymer crystals. Porous spheres based on crystalline PLLA were observed on the upper face, because they were more resistant to enzymatic attack. The crystallinity of the films increased monotonously with the hydrolysis time, thus, the absorption of water gradually decreased. The analysis of degradation residues revealed that many colloids of poly(2-ethyl-2-oxazoline)-co-polyethylenimine (PEOz-co-PEI) copolymers were dispersed in the buffer solution. The average diameter, 1 mum, of the colloids was reduced to 200 nm by advanced degradation. The proteinase K exhibited remarkable hydrolysis not only at the ester bond but also the amide bond. (C) 2004 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据