4.8 Article

Reduction and adsorption mechanisms of selenate by zero-valent iron and related iron corrosion

期刊

APPLIED CATALYSIS B-ENVIRONMENTAL
卷 104, 期 1-2, 页码 185-192

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.apcatb.2011.02.014

关键词

Selenate; ZVI; XANES and EXAFS spectroscopy; XRD; Magnetite; Lepidocrocite

资金

  1. GIST
  2. MEST
  3. POSTECH

向作者/读者索取更多资源

The mechanisms of selenate [Se(VI)] removal by zero-valent iron (ZVI) were investigated using X-ray absorption spectroscopy (XAS) including X-ray absorption near-edge structure (XANES) and extended X-ray absorption fine structure (EXAFS) spectroscopy, X-ray diffraction (XRD), and scanning electron microscopy (SEM). Batch experiments were performed to measure the ZVI removal of Se(VI) as a function of Se(VI) concentration, pH, and dissolved oxygen (DO) concentration; these experiments demonstrated that low Se(VI) concentration, low pH, and the presence of DO increased the kinetics of Se(VI) removal. XAS showed that the main factor affecting Se(VI) reduction and adsorption as well as ZVI corrosion was the ratio between Se(VI) concentration and ZVI. At high Se(VI) concentrations (>50 mg/L), lepidocrocite (gamma-FeOOH) was the principal ZVI corrosion product. During ZVI corrosion, Se(VI) was not completely reduced to Se metal [Se(O)]/selenide [Se(-II)] with 1 g/L ZVI, although Se(VI)/selenite [Se(IV)] was adsorbed onto the surface of the lepidocrocite. At a low Se(VI) concentration (10 mg/L), Se(VI) was reduced to Se(0)/Se(-II) with 1 g/L ZVI, which indicated that reduction by ZVI was the principal mechanism of Se(VI) removal, with magnetite (Fe3O4) being the primary corrosion product in the absence of absorbed Se(VI) ions. Therefore, the reduction capacity and iron corrosion coating of ZVI depended on Se(VI) concentration (i.e., the Se(VI)/ZVI ratio) and less extensively on pH and DO. (C) 2011 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据