期刊
APPLIED CATALYSIS B-ENVIRONMENTAL
卷 78, 期 1-2, 页码 166-175出版社
ELSEVIER SCIENCE BV
DOI: 10.1016/j.apcatb.2007.09.024
关键词
aluminium foams; anodisation; zeolite washcoating; catalyst coating adhesion
The anodisation conditions of aluminium foam monoliths are studied in order to produce alumina with controlled properties. When anodisation conditions are extreme, an important cracking of the surface appears with width and depth cracks that depend on the anodisation parameters, i.e., electrolyte temperature, anodisation time and applied current density. Different surface treatments for aluminium foams (rough anodisation, smooth anodisation, and no anodisation) were used to observe the mechanical stability of Pt/ZSM5 coatings. Roughness of the surface improved adhesion of Pt/ZSM5 coatings because the size of the cracks was high enough to occlude the zeolite particles promoting a mechanical anchorage of the coating. The washcoated aluminium foam monoliths were tested in total oxidation of toluene showing very high activity. (C) 2007 Elsevier B.V. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据