4.6 Article

Synthesis, characterization and catalytic activity of ruthenium-doped cobalt catalysts

期刊

APPLIED CATALYSIS A-GENERAL
卷 341, 期 1-2, 页码 35-42

出版社

ELSEVIER
DOI: 10.1016/j.apcata.2007.12.034

关键词

mesoporous MSU; cobalt catalysts; tetralin hydrogenation; hydrogenolysis/hydrocracking; sulphur tolerance

向作者/读者索取更多资源

Cobalt-based catalysts doped with different amounts of ruthenium supported on Zr-MSU type materials were studied in the hydrogenation and hydrogenolysis/hydrocracking of tetralin at different temperatures. The catalytic tests were carried out in a high-pressure fixed-bed continuous-flow stainless steel catalytic reactor operating at a pressure of 6.0 MPa. Textural, structural, acidic and metallic properties were studied by XRD, XPS, H-2-TPR, NH3-TPD and Elemental Chemical Analysis. Five catalysts were prepared with 10 wt% of cobalt and a ruthenium loading ranging from 0.5 to 5 wt%, along with a monometallic ruthenium catalyst with 3 wt% of metal, for comparison. From catalysts characterization, no interaction between cobalt and ruthenium can be established, however, the presence of ruthenium influences the reducibility of cobalt. Ruthenium-doped catalysts not only improve the catalytic activity of monometallic cobalt and ruthenium ones, but also ruthenium acts as a trap for sulphur organic molecules, preserving cobalt particles from sulphur poisoning and thus maintaining their high hydrogenation activity. The catalyst with a ruthenium loading of 3 wt% is found to be the most active, both, with or without sulphur in the feed. The most striking improvement of ruthenium-doped catalyst properties is their greater resistance to sulphur molecules than in the case of monometallic cobalt catalysts, which are otherwise rapidly deactivated under the same experimental conditions. (c) 2008 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据