期刊
PARTICULATE SCIENCE AND TECHNOLOGY
卷 23, 期 3, 页码 265-284出版社
TAYLOR & FRANCIS INC
DOI: 10.1080/02726350590955912
关键词
particle size distribution (PSD); image analysis (IA); laser diffraction (LD); ultrasonic attenuation spectroscopy (UAS); focused-beam reflectance measurement (FBRM); chord length distribution (CLD)
In this article, particle size distributions (PSDs) measured by different techniques, including image analysis (IA), laser diffraction (LD), ultrasonic attenuation spectroscopy (UAS), and focused-beam reflectance measurement (FBRM), are compared for spherical glass beads and nonspherical silica flakes. It is shown that particle shape strongly affects the results obtained by different techniques. For spheres, the PSDs obtained by IA, LD, and UAS agree well. There is no consistent result among different particle measurement techniques for nonspherical particles. The conversion between PSDs obtained by IA, LD, and UAS has been based on particle shape factors. Caution must be exercised when a measured chord length distribution (CLD) is used to indicate the PSD during a process because the CLD result obtained by FBRM is complex, depending not only on the PSD, but also on particle optical properties and shape.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据