thermoelectric property; Bi2Te3; hot-pressing; phonon scattering
Fine-grained Bi2Te3 alloys have been prepared by a hot-pressing method using Bi2Te3 particles with an average particle size of 150 nm. The fine Bi2Te3 powders were synthesized by a hydrogen-reduction method using coprecipitation. In order to investigate the effects of phonon-grain boundary scattering, the grain size of hot-pressed alloys was controlled between 1.2 and 3.9 mu m by hot-pressing time. The Hall coefficient and the thermoelectric properties were measured in the temperature range 200-300 K. The thermoelectric properties of the hot-pressed samples were investigated from the view points of their grain size dependence and carrier concentration. It was found that the lattice thermal conductivity for an average grain size of 1.2 mu m was reduced by about 60% compared with a single crystal of Bi2Te3 due to phonon-grain boundary scattering. Also, the grain size dependence of the thermoelectric properties was discussed. (c) 2005 Elsevier B.V. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据