4.6 Article

Mechanical properties of retrieved highly cross-linked crossfire liners after short-term implantation

期刊

JOURNAL OF ARTHROPLASTY
卷 20, 期 7, 页码 840-849

出版社

CHURCHILL LIVINGSTONE INC MEDICAL PUBLISHERS
DOI: 10.1016/j.arth.2005.07.015

关键词

mechanical properties; oxidation; wear; hip arthroplasty; highly cross-linked ultra-high-molecular-weight polyethylene

资金

  1. NIAMS NIH HHS [R01 AR047904, R01 AR47904] Funding Source: Medline

向作者/读者索取更多资源

This study reports on detailed analyses of retrieved, annealed cross-linked liners. Twelve cross-linked liners (Crossfire, Stryker Orthopaedics, Mahwah, NJ) of the same Omnifit design were retrieved at revision surgery by one institution after an average 1.9 years (0.02-4.8 years) in vivo. In each case, the revision surgery was performed for reasons unrelated to wear. The mechanical properties and extent of oxidation of all inserts were characterized using a standard small punch test and measurement of the oxidation index. Results indicated that there was no association between implantation time and either mechanical properties or extent of oxidation for the inserts near the worn bearing surface. Slight variation in properties was observed as a function of sampling location, with the properties near the unworn surface displaying the greatest relative variability. We conclude that the variability in polyethylene properties observed in this small study was not clinically significant for these short-term-implanted, annealed cross-linked liners.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据