Evolution of inclusions and resultant microstructural change with Mg addition in Mn/Si/Ti deoxidized steels

期刊

SCRIPTA MATERIALIA
卷 53, 期 11, 页码 1253-1258

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.scriptamat.2005.08.001

关键词

oxides; dispersion of non-metallic particles; interface wetting; grain refining

向作者/读者索取更多资源

Evolution of non-metallic inclusions with Mg addition in Mn/Si/Ti deoxidized steels was analyzed focusing on their phase, composition, size, and number density. The changes in the size and the number density were discussed in terms of the wettability of inclusions with melt, and correlated with the as-cast microstructures of steels. (c) 2005 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.