Viscosity measurements of Zr55Cu30Al10Ni5 and Pd40Cu30Ni10P20 supercooled liquid alloys by using a penetration viscometer

期刊

MATERIALS TRANSACTIONS
卷 46, 期 12, 页码 2746-2750

出版社

JAPAN INST METALS & MATERIALS
DOI: 10.2320/matertrans.46.2746

关键词

Zr55Cu30Al10Ni5; Pd40Cu30Ni10P20; supercooled liquid; penetration viscometer; oxygen contamination; activation energies

向作者/读者索取更多资源

Viscosity of Zr55Cu30Al10Ni5 and Pd40Cu30Ni10P20 supercooled liquid alloys having bulk metallic glass forming ability has been measured by using a penetration viscometer with a cylindrical probe under high speed heating conditions at heating rates between 20 and 400 degrees C/min in the temperature range from the glass transition temperatures (T-g) up to above the crystallization temperatures. The viscosity of these alloys decreased with increasing the heating rate and tended to saturate at the heating rate of 200 degrees C/min and above. Their viscosity could be well represented by the Arrhenius relation. The activation energies for viscous flow for Zr55Cu30Al10Ni5 and Pd40Cu30Ni10P20 supercooled liquid alloys were about 350 and 250 kJ/mol, respectively. The viscosity was also fitted by a Vogel-Fulcher-Tammann (VFT) relationship over the entire temperature range.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据