期刊
JOURNAL OF POWER SOURCES
卷 153, 期 2, 页码 360-364出版社
ELSEVIER
DOI: 10.1016/j.jpowsour.2005.05.037
关键词
gel polymer electrolyte; lithium/sulfur batteries; tetraglyme; discharge process
The Li/PVdF/S cell showed the first discharge capacity of 1268 mAh g(-1), which was about 78% utilization of theoretical value. There were two plateau regions at the first discharge curve. From the XRD, DSC results of the sulfur electrode, elemental sulfur disappeared at the upper plateau region and Li2S was formed at the low plateau region. We suggested the discharge process of Li/polymer electrolyte/S cell. The elemental sulfur changed into Li2Sn (n > 4) and subsequently changed into Li2S at a lower plateau potential region. (c) 2005 Elsevier B.V. All rights reserved.