4.4 Article

Effects of molten salt synthesis (MSS) parameters on the morphology of Sr3Ti2O7 and SrTiO3 seed crystals

期刊

JOURNAL OF ELECTROCERAMICS
卷 16, 期 2, 页码 159-165

出版社

SPRINGER
DOI: 10.1007/s10832-006-6243-2

关键词

molten salt synthesis; Sr3Ti2O7; SrTiO3; seed crystals; texturing

向作者/读者索取更多资源

A two-step molten salt synthesis process was utilized to fabricate Sr3Ti2O7 and SrTiO3. High aspect ratio SrTiO3 seed crystals were developed by optimizing processing conditions such as temperature, salt-to-oxide ratio, and flux type in a systematic fashion. Sr3Ti2O7 seeds were synthesized at temperatures ranging from 1050-1350 degrees C, using salt-to-oxide ratios of 3:1, 1:1, and 1:3, and various salt types, including NaCl, KCl, and a 1:1 combination of NaCl and KCl. Sr3Ti2O7 seeds synthesized at 1250 degrees C with a 1:1 salt-to-oxide ratio in 100% NaCl salt resulted in a majority of higher aspect ratio platelets and elongated platelets as opposed to lower aspect ratio cubic-like and tetragonal-like morphologies. The seeds were 10-40 mu m in length with aspect ratios of highly elongated platelets as high as 25:1. A second MSS step was used to synthesize SrTiO3 seeds of the proper composition by TiO2 addition to the Sr3Ti2O7 seeds and heat treatment at 1100 degrees C. These studies showed that highly anisotropic SrTiO3 seeds could be produced at 1250 degrees C using a 1:1 salt-to-oxide ratio in 100% NaCl flux. XRD studies of the resulting SrTiO3 seeds revealed that the increase in aspect ratio for these particular seeds also resulted in the enhancement of (200) peaks, which are of major interest for texturing of PMN-PT.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据