The effect of some fillers on PVC degradation

期刊

JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS
卷 75, 期 2, 页码 112-119

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jaap.2005.04.012

关键词

PVC degradation; hydrogen chlorine absorber; Red Mud; carbonates

向作者/读者索取更多资源

The HCl scavenging effect of particulate fillers such as Red Mud (RM), CaCO3 and dolomite on the thermal degradation of PVC was investigated by thermogravimetry/mass spectrometry (TG/MS). It was found that, in the presence of carbonates, the peak temperature (T-max) of dehydrochlorination was shifted to a higher temperature and the rate of mass loss was decreased, while, in the presence of M FeCl3 was formed and dehydrochlorination of PVC was accelerated, but the second decomposition step of PVC has been retarded. Benzene formation has been hindered by the acid scavenger additives and retarded by RM, evolution of benzene and other aromatics being shifted to higher temperatures. (C) 2005 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据