期刊
JOURNAL OF MATERIALS IN CIVIL ENGINEERING
卷 18, 期 2, 页码 161-174出版社
ASCE-AMER SOC CIVIL ENGINEERS
DOI: 10.1061/(ASCE)0899-1561(2006)18:2(161)
关键词
-
This paper examines the compressibility and strength characteristics of high water content cement-admixed clay in deep mixing applications. During curing time, both cement content and total clay water content of the clay-water-cement mixture significantly affect the strength and compressibility of the resulting stabilized clay. To ensure optimum improvement, the selection of an appropriate total clay water content for a mixture with a certain cement content is crucial. Furthermore, the fundamental parameters such as the ratio of after-curing void ratio (e,) and cement content (A,,,) have been found sufficient to characterize the strength and compressibility of cement-admixed clay. The results of unconfined compression and consolidated-undrained tests have proven that the ratio e(ol)/A(w) combines to-ether the influences of clay water content, cement content, and curing time as well as curing pressure on the strength of cement-admixed clay. In addition, useful empirical relationships on deep mixing application are presented.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据