Kelvin probe force microscopy on surfaces of UHV cleaved ionic crystals

期刊

NANOTECHNOLOGY
卷 17, 期 7, 页码 S155-S161

出版社

IOP Publishing Ltd
DOI: 10.1088/0957-4484/17/7/S09

关键词

-

向作者/读者索取更多资源

Force spectroscopy and Kelvin probe force microscopy (KPFM) measurements taken on (001) Surfaces of UHV cleaved NaCl, KCl and MgO are presented for the first time. With the help of force spectroscopy we show first that the charging of (001) surfaces of alkali halide crystals, which generally occurs after UHV cleavage, vanishes after a couple of days due to their sufficiently high ionic conductivity at room temperature. KPFM images of these (001) surfaces show that the surface potential is not uniform but exhibits variations of up to 1 V at a nanometre length scale. Variations oil terraces as well as a strong contrast at step edges can be observed, of which the latter is probably due to trapped charges. On MgO(001), we observe strong changes in the surface potential, especially at previously reported adstructures. These changes explain why imaging MgO(001) is difficult.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据