INTERMETALLICS
卷 14, 期 6, 页码 603-606出版社
ELSEVIER SCI LTD
DOI: 10.1016/j.intermet.2005.10.003
关键词
nickel aluminides; based on NiAl; composites; sintering
The paper presents the results of examinations of the NiAl-Al2O3 sinters (13, 38 and 55 vol% of Al2O3) produced from a mixture of nickel, aluminum and alumina powders in a single technological process, using the pulse plasma sintering (PPS) method. By subjecting the elemental powders to a PPS process for 900 s, we obtained NiAl-Al2O3 composites of a hardness ranging from 480 HV10 (13% Al2O3) to 680 HV10 (55% Al2O3). The fracture toughness of the sintered materials depended on the amount of the dispersed Al2O3 phase. When examined with a Vickers indenter under a load of 10 kg, the composite containing 13% of Al2O3 showed no cracking. In the composites with 38% Al2O3 and 55% Al2O3 contents, the value of K-IC was 9.1 and 8.2 MPam(1/2), respectively. (c) 2005 Published by Elsevier Ltd.