期刊
MATERIALS LETTERS
卷 60, 期 12, 页码 1554-1557出版社
ELSEVIER SCIENCE BV
DOI: 10.1016/j.matlet.2005.11.090
关键词
SnO2; varistors; microstructure; electrical properties
The variation of the electrical properties of a well-known tin oxide varistor composition in relation to the sintering time for temperatures of 1300 and 1350 degrees C was studied in this work. It was verified that the barrier voltage value, nu(b), varies according to the varistor sintering time. Stable electrical barriers between 2.0 and 2.4 V/barrier produce varistors with non-linear coefficients higher than 35, independently of the sintering temperature. The variation of the grain size in relation to the sintering time was 45.1% for sintering at 1300 degrees C and 33.6% for sintering at 1350 degrees C, considering the minimum time of I h and the maximum of 12 h, with considerable variations in the respective electrical breakdown fields. Therefore, the sintering time is a very important variable which should not be despised in the project of tin oxide varistor production. (c) 2006 Published by Elsevier B.V.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据