Bismuth telluride based n-type thermoelectric materials were prepared via the route of mechanical alloying (MA) and subsequent hot pressing (HP) process. Influence of hot press process parameters on the thermoelectric properties was investigated. Increasing hot pressing temperature from 340 to 400 degrees C, the figure of merit of the hot pressed sample increases rapidly, and then it grows slowly and no improvement is obtained when further increasing from 460 to 500 degrees C. Prolonging hot pressing time appropriately is helpful to improve thermoelectric properties, a maximum figure of merit of 1.7 x 10(-3) K-1 has been obtained for the 4 h HP-ed sample. (c) 2005 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据