Transparent YAG ceramics by surface softening of nanoparticles in spark plasma sintering

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.msea.2006.04.072

关键词

densification; spark plasma sintering (SPS); ceramic; grain growth; nanoparticle; YAG

向作者/读者索取更多资源

Rapid heating of 34 nm yttrium aluminum gamet (YAG) nanoparticle compacts using pulsed high direct electric current, during the spark plasma sintering (SPS), resulted in transparent ceramics, after 3 min at 100 MPa and 1400 degrees C. This phenomenon is in contrast to conventional sintering at much higher temperatures that result in translucent or opaque ceramics. Grain growth analysis and the evolved microstructure during the SPS showed that the YAG nanoparticle surfaces soften due to the pulsed direct electric current. Dynamic densification to transparency occurs by nanograin rotation and sliding, aided by the viscous layer, and followed by curvature driven grain boundary diffusional processes at higher densities and grain sizes. (c) 2006 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据