4.7 Article Proceedings Paper

Effect of surface OH groups on catalytic performance of yittrium-stabilized ZrO2 in partial oxidation of CH4 to syngas

期刊

CATALYSIS TODAY
卷 117, 期 1-3, 页码 163-167

出版社

ELSEVIER
DOI: 10.1016/j.cattod.2006.05.046

关键词

partial oxidation of methane; yittrium-stabilized ZrO2; surface hydroxyl groups; formaldehyde

向作者/读者索取更多资源

The influence of water and surface hydroxyl groups on the catalytic performance of yittrium-stabilized ZrO2 (YSZ) in the partial oxidation of methane to synthesis gas was investigated using FT-IR as well as steady state kinetic experiments. Besides physically adsorbed water, terminal OH groups, bi-bridging and tri-bridging OH groups exist on the surface of YSZ. Oxidation of formaldehyde to formate, occurs on the low index planes rather than at the structural defects, i.e. corners, edges, kinks and steps. Adsorbed formaldehyde is attacked by neighboring lattice oxygen ions in low index surface planes to form surface formate. Neighboring hydroxyl groups and hydrogen-bonded molecular water on the surface of YSZ suppress this nucleophilic attack. In short, the presence of water on the surface stabilizes adsorbed formaldehyde, decreasing the rate of oxidation to formate; this effect is responsible for the increase in selectivity to H-2 and CO when water is added during CPO. (C) 2006 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据