Fabrication of polyaniline nanostructures under ultrasonic irradiation: From nanotubes to nanofibers

期刊

MACROMOLECULAR CHEMISTRY AND PHYSICS
卷 207, 期 22, 页码 2142-2152

出版社

WILEY-V C H VERLAG GMBH
DOI: 10.1002/macp.200600424

关键词

dopant acid; nanofibers; nanotubes; polyaniline; ultrasonic irradiation

向作者/读者索取更多资源

An ultrasonic irradiation assisted polymerization method has been used to prepare PANI nanotubes and nanofibers by using different doping concentrations of mineral or organic acids. It has been found that PANI nanotubes can be produces when the concentration of the dopant acid is low. However, PANI nanofibers can also be produced when the concentration of the dopant acid is high. Foe nanotubes synthesized at a low concentration of the dopant acid, the outer average diameter can be changed from about 150 nm using phospheric acid to 200 nm using nitric acid as the dopant and the inter diameter is in the range from about 50 nm using nitric acid to more than 110 nm using perchloric acid as the dopant. The mechanism of the formation of the nanotubes and nanofibers may be due to the formation of different kinds of micelles and the prevention of the second growth of the PANI by ultrasonic irradiation. The chemical structure of the PANI nanotubes and nanofibers are characterized by FTIR and UV-vis absorption spectra and XRD patterns. The conductivity of the PANI nanofibers is comparable to that of conventional PANI samples.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据