The basis for a second-generation highly cross-linked UHMWPE

期刊

CLINICAL ORTHOPAEDICS AND RELATED RESEARCH
卷 -, 期 453, 页码 265-271

出版社

LIPPINCOTT WILLIAMS & WILKINS
DOI: 10.1097/01.blo.0000238856.61862.7d

关键词

-

向作者/读者索取更多资源

Highly cross-linked ultra-high molecular weight polyethylene (UHMWPE) decreases wear at the hip by more than 50% compared with conventional UHMWPE. However, melted highly cross-linked polyethylene may be susceptible to fatigue cracking, and annealed highly cross-linked polyethylene may be susceptible to in vivo oxidation. The second-generation highly cross-linked UHMWPE (X3 HXPE) uses a sequential irradiation and annealing process. It preserves mechanical strength properties and has the highest survivor-ship in functional fatigue testing. The free radical content is low, and its performance under accelerated aging is the same as virgin UHMWPE. Hip simulator studies with 32-mm acetabular components demonstrated 97% wear reduction compared with conventional UHMWPE, and 62% compared with a clinically successful first-generation annealed highly cross-linked polyethylene. The crystallinity, density, and tensile strength of the X3 HXPE material was unchanged by oxidative challenge. X3 HXPE material articulating on co-balt-chromium alloy yields a volumetric wear rate very similar to that of metal-on-metal articulations, but eliminates the concerns of metal ion release. Wear particles generated from the X3 HXPE were the same size as those produced from conventional UHMWPE. Preliminary results suggest X3 HXPE can be used for cups larger than 36 mm.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据