Synthesis and characterization of Co3O4 hollow spheres

期刊

MATERIALS LETTERS
卷 61, 期 3, 页码 701-705

出版社

ELSEVIER
DOI: 10.1016/j.matlet.2006.05.046

关键词

Co3O4; hollow spheres; surfactant; hydrothermal synthesis

向作者/读者索取更多资源

Co3O4 hollow spheres were hydrothermally prepared at 130 degrees C for 16 h in the presence of Poly-vinylpyrrolidone (PVP). The as-prepared products were characterized by powder X-ray diffraction (XRD), field-emission scanning electron microscope (FE-SEM), transmission electron microscopy (TEM), infrared spectrum (IR), X-ray photoelectron spectrum (XPS), and optical absorption spectrum. PVP surfactant plays important roles in the formation of Co3O4 hollow spheres. These Co3O4 hollow spheres have average diameters of ca. 350 nm, and the wall thickness around the shell is about 42 nm. The possible formation mechanism of hollow Co3O4 spherical structures has simply been proposed. (c) 2006 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据